35CrMov alloy steel bar

  • 273 Views
  • 11-May-2024

35CrMoV alloy structural steels. Unified digital code: A31352
Standard: GB / T 3077-1988

35CrMoV alloy chemical composition:

C

Si

Mn

S

P

Cr

Ni

Cu

V

Mo

0.30~0.38

0.17~0.37

0.40~0.70

≤0.035

≤0.035

1.00~1.30

≤0.030

≤0.030

0.10~0.20

0.20~0.30

35CrMoV alloy mechanical properties:
Blank sample size (mm): 25 Heat treatment : the first quenching temperature (℃): 900; Coolant: Oil
The second quenching temperature (℃): tempering heating temperature (℃): 630; Coolant: water, oil
Tensile strength σb (MPa): ≥ 1080 (110) Yield strength σs (MPa): ≥ 930 (95)
Elongation δ5 (%): ≥ 10 Reduction of area ψ (%): ≥ 50
Impact energy Akv (J): ≥ 71 Impact toughness values ​​αkv (J/cm2): ≥ 88 (9)
Brinell hardness (HBS100/3000) ( annealing or tempering state ): ≦ 241 [2] Delivery Status

Delivery status : to heat treatment ( normalizing, annealing or tempering ) or without heat treatment delivery , the delivery status should be specified in the contract.

35CrMoV alloy representation:
① steel beginning of a two-digit number indicates the carbon content of steel to the average carbon content of the few that, as 40Cr, 25Cr2MoVA alloy tube
② main alloying elements in steel , in addition to individual micro- alloying elements , typically a few percent . When the average alloy content < 1.5% , steel generally mark the element symbol not indicate the content , but prone to cause confusion in exceptional circumstances , after the element symbol can also be marked with the number "1" , such as steel "12CrMoV" and "12Cr1MoV", the former chromium content of 0.4-0.6 % and 0.9-1.2 % , the remaining ingredients are all the same . When the average content of alloying elements ≥ 1.5%, ≥ 2.5%, ≥ 3.5% ...... when , after the element symbol should be marked content, can be expressed as the corresponding 2,3,4 ...... and so on. For example 18Cr2Ni4WA.
③ Steel Vanadium V, Ti Ti, Al AL, boron B, RE alloys of rare earth elements are micro-alloying elements , although the content is very low , the steel should bid out . For example 20MnVB steel. 0.07-0.12 % vanadium , 0.001 to 0.005 % of boron .
④ High quality steel should finally add "A" in the steel , as distinct from the general high quality steel .

⑤ special purpose , steel, known ( or suffix ) represents the symbol of the steel purposes. For example riveting Lo dedicated 30CrMnSi steel, steel represented as ML30CrMnSi.

Alloy steel pipe is produced in accordance with the material ( ie material ) to define , as the name suggests is made ​​alloy tubes ; and seamless steel pipe according to the production process (with seam seamless ) to define , is different from the seamless pipe joints, including the Longitudinal and spiral

Related Post

API5L X60 PSL1 LSAW steel pipeline

API5L X60 PSL1 LSAW steel pipeline has minimum yield strength and minimum ultimate tensile strength.

DNV EH40 shipbuilding steel plate

DNV EH40 shipbuilding steel plate is a kind of hot rolled high tensile strength steel. Higher-strength DNV shipbuilding steel comes in 12 grades of 3 strengths, DNV EH40 shipbuilding steel plate is one of the grades. The DNV EH40 shipbuilding steel plate

DX53D Galvanized Steel Pipe

KUNFENG Steel can cut to the size you need and supply galvanized steel pipes in various grades, sizes, and thicknesses. Our extensive galvanized steel pipe inventory can efficiently meet your most challenging custom galvanized steel pipe needs.

GL Grade B shipbuilding steel plate

GL Grade B shipbuilding steel plate is a kind of hot rolled general tensile strength steel. The GL shipbuilding steel plate have yield strength of 34,100 psi (235 MPa), and ultimate tensile strength of 58,000 - 75,500 psi (400-520 MPa).