ISO3183 L450M/X65M PSL2 LSAW pipeline used in natural gas pipeline, petroleum, chemical, water, we are the manufacturer and supplier in China, can provide a large number of high quality ISO3183 L450M/X65M PSL2 LSAW pipeline spot,and can carry out chemical composition analysis, mechanical properties, external inspection, X-ray test, X-ray test and a series of tests.

ISO3183 L450M/X65M PSL2 LSAW pipeline Chemical Composition :

Grade

Chemical composition %  (Max)

C

Si

Mn

P

S

V

Nb

Ti

L450M/X65M

0.12

0.45

1.60

0.025

0.015

-

-

-

ISO3183 PSL2 L450M/X65M Mechanical Properties

Grade

Mechanical properties

Yield Strength (Mpa)

Tensile Strength(Mpa)

L450M/X65M

450-600

535-760

The above is our ISO3183 L450M/X65M PSL2 LSAW pipeline related performance and application, if you also want to know more, please feel free to contact us, we will take strict product quality supervision to ensure that the flow into our target market is not inferior to ISO3183 L450M/X65M PSL2 LSAW pipeline products. You are welcome to inquire.

Related Post

API 5L Gr.B PSL1 LSAW steel Pipeline

API 5L Gr.B PSL1 steel Pipeline for use in pipeline transportation systems in the petroleum and natural gas industries ;predominantly used in the construction of chemical plant, vessels, pipe work and for general mechanical engineering purposes.

API 2W Gr.50/Gr.60 steel work / steel structure / steel machining parts

KUNFENG have been playing vital supplier role in the full spectrum of industries ranging from oil and gas,power plant,cement plant,shipbuilding,bridge,building,crane building etc.

55# hot rolled round bars and forged round bars

55# hot rolled and forged round bars are fine carbon structural steel under the standard of GB/T 699-1999 After treating,55# hot rolled and forged round bars, with high surface hardness and strength, but low plasticity and toughness.

ABS AH32 shipbuilding steel plate

The ABS AH32 shipbuilding steel plates have yield strength of 45,500 psi (315 MPa), and ultimate tensile strength of 64,000 - 85,000 psi (440-590 MPa).